Design basis of LPG tank powder coating line
1. Name of workpiece: LPG tank
2. Max size of LPG tank: Diameter: 440mm Height: 1200mm
3. Max hanging size on each hanger: L500mm×W500mm×H1500mm
4. Loading capacity on hanging hook: ≤35kg
5.Suggested interval between 2 hangers: 300mm
6. Conveying speed: 1m/min
7.Output: 60-75pcs per hour
8. Spraying method: 4 auto spray guns (match on 1 reciprocator) & 1 manual spray gun
9. Heating source: natural gas (Other choices are available: electricity, oil or coal)
10. Pretreatment system: immersion tank type
11. Required plant size: L52m×W28m×H6.5m
Design description for LPG cylinder powder painting line
1. According to the shape of LPG tank, we design the pretreatment to be
economical immersion tank type with 6 stage processings.
2. After chemical cleaning, he pre-treated workpieces will be conveyed to drying furnace
for water removal on their surface. The drying furnace is designed
being tank type to match with immersion pretreatment tanks, and with a
top-door design for easy access of pre-treated workpieces.
3. After drying, the workpieces are ready for powder particle adhesion. Please manually feed them on auto powder painting line. For a better painting result, the spray booth, waster powder recycling system,
reciprocator adopts advanced equipments in China through our careful
selection. And the spraying guns, both auto and manual are imported
from foreign famous company for a longer service life. Then these
workpieces will be sent to gas-fired furnace tunnel to let powder melt
into a smooth coating.
Process flow for LPG holder powder coating line
1. Feed your LPG tank on crane hanger for the preparation for chemical cleaning
2. Pre-degreasing stage
3. Degreasing stage
4. Rinsing stage
5. Surface conditioning stage
6. Phosphating stage
7. Rinsing stage
8. Drying off oven to remove surface moisture (100-120℃ for 10 mins)
9. Manually transfer the pre-treated objects to powder coating line
10. Powder application with spray guns
11. Powder curing (180-200 ℃ for 20 mins)
12. Finished product discharging